Skip to main navigation Skip to main content
  • KIEEME

J Electr Electron Mater : Journal of Electrical and Electronic Materials

OPEN ACCESS
ABOUT
BROWSE ARTICLES
EDITORIAL POLICIES
FOR CONTRIBUTORS

Page Path

3
results for

"LN2"

Keywords

Publication year

Authors

"LN2"

High Voltage and Discharge Engineering : Correlation Analysis of the Dielectric Breakdown Voltage of Liquid Nitrogen
Seung Myeong Baek
J Korean Inst Electr Electron Mater Eng 2015;28(6):396-399.   Published online June 1, 2015
DOI: https://doi.org/10.4313/JKEM.2015.28.6.396
We analyzed the correlation between breakdown voltage(BDV) of liquid nitrogen(LN2) and factors. The chosen factors affecting the breakdown are the diameter of electrode, gap length, temperature of LN2, and pressure of LN2. The BDV of LN2 was increased with increasing the diameter, the gap length and the pressure. And The BDV of LN2 was increased with decreasing the temperature. However, correlation coefficient was different from each other depending on the situation. The BDV exhibited a very high correlation coefficient of 0.92227 to dependence on the diameter. And a very high correlation coefficient of 0.94980 to dependence on the pressure under sphere(D 7.5 mm)-plane electrode. When the pressure is applied, sphere-plane electrode is the correlation coefficient was higher than that of the needle-plane electrode. It shows the dependence of a temperature coefficient of ?0.758290 ~ -0.39946 under needle-plane electrode.
  • 64 View
  • 0 Download
High Voltage and Discharge Engineering : Shape and Dielectric Strength of Thermal Bubbles in Liquid Nitrogen
Seung Myeong Baek, Hae Jong Kim
J Korean Inst Electr Electron Mater Eng 2015;28(5):326-331.   Published online May 1, 2015
DOI: https://doi.org/10.4313/JKEM.2015.28.5.326
In this paper, we study the insulating properties of the liquid nitrogen(LN2) including the thermal bubbles. The shape of the thermal bubbles in accordance with the current change was observed in the 77 K and 65 K LN2. According to the temperature of liquid nitrogen, bubbles were generated differently. The round shape of the bubble is occurred in 77 K LN2. But the layer shape of bubble is occurred in 65 K LN2. When the bubbles present, the dielectric strength of liquid nitrogen is low. However, the breakdown patterns were different according to the electrode arrangement. AC breakdown voltage(BDV) was lower than the DC BDV due to the influence of bubbles. Therefore, the design of a high-voltage superconducting equipments should consider the bubbles.
  • 61 View
  • 0 Download
Bending Strain Dependence of the Critical Current in Externally-reinforced Bi-2223 Tapes with Different Hermeticity under pressurized Liquid Nitrogen